10 Common Problems and Solutions in Deep Hole Machining


Release time:

2020-12-14

【Summary】In the deep hole machining process, issues such as the dimensional accuracy of the workpiece, surface quality, and tool life often arise. How to reduce or even avoid these problems is a pressing issue we need to address. 1. Increased hole diameter, large error 1) Causes The design value of the reamer's outer diameter is too large or the cutting edge has burrs; cutting speed is too high; improper feed rate or excessive machining allowance; the main angle of the reamer is too large; the reamer is bent; chips adhere to the cutting edge; the runout of the cutting edge during grinding exceeds the limit; inappropriate selection of cutting fluid; oil stains on the conical surface of the reamer are not cleaned before installation, or the conical surface has bumps; the flat tail of the conical shank is misaligned when installed in the machine spindle, causing conical interference; spindle bending or spindle bearings are too loose or damaged; the reamer floats ineffectively; misalignment with the workpiece and uneven force applied by both hands when hand reaming, causing the reamer to sway left and right. 2) Solutions Appropriately reduce the outer diameter of the reamer according to the specific situation; lower the cutting speed; adjust the feed rate or reduce the machining allowance; appropriately reduce the main angle; straighten or scrap bent reamers that cannot be used; carefully grind to meet standards with an oil stone; control runout within allowable limits; choose cutting fluids with good cooling performance; before installing the reamer, clean the oil stains on the conical shank and the inside of the machine spindle's conical hole, and polish any bumps on the conical surface with an oil stone; grind the flat tail of the reamer; adjust or replace spindle bearings; readjust the floating chuck and adjust coaxiality; pay attention to correct operation. 2. Decreased hole diameter 1) Causes The design value of the reamer's outer diameter is too small; cutting speed is too low; feed rate is too high; the main angle of the reamer is too small; inappropriate selection of cutting fluid; during grinding, the worn part of the reamer is not ground off, causing elastic recovery that reduces the hole diameter; when reaming steel parts, excessive allowance or dull reamer can easily cause elastic recovery, leading to reduced hole diameter and non-circular inner holes, resulting in unqualified hole diameter. 2) Solutions Replace the outer diameter of the reamer; appropriately increase the cutting speed; appropriately reduce the feed rate; appropriately increase the main angle; choose lubricating cutting fluids; regularly interchange reamers and correctly grind the cutting part of the reamer; when designing the reamer size, consider the above factors or take values based on actual conditions; conduct experimental cutting, take appropriate allowances, and sharpen the reamer. 3. Non-circular inner holes 1) Causes The reamer is too long, lacks rigidity, and vibrates during reaming; the main angle of the reamer is too small; the cutting edge is too narrow; the allowance for the reamed hole is off; the inner hole surface has notches or cross holes; the hole surface has sand holes or air holes; spindle bearings are loose, there is no guide sleeve, or the gap between the reamer and the guide sleeve is too large, and due to tight clamping of thin-walled workpieces, deformation occurs after removal. 2) Solutions For reamers with insufficient rigidity, use reamers with unequal tooth pitch, and install the reamer using a rigid connection, increasing the main angle; select qualified reamers and control the hole position tolerance in the pre-processing stage; use reamers with unequal tooth pitch and longer, more precise guide sleeves; select qualified blanks; when reaming precise holes with equal tooth pitch reamers, adjust the machine spindle's gap, and the fit gap of the guide sleeve should be high or use appropriate clamping methods to reduce clamping force. 4. Obvious edges on the inner surface of the hole 1) Causes Excessive allowance for the reamed hole; the back angle of the cutting part of the reamer is too large; the cutting edge is too wide; the workpiece surface has air holes, sand holes, and excessive spindle runout. 2) Solutions Reduce the allowance for the reamed hole; reduce the back angle of the cutting part; grind the width of the cutting edge; select qualified blanks; adjust the machine spindle. 5. High roughness value of the inner hole surface 1) Causes Cutting speed is too high; inappropriate selection of cutting fluid; the main angle of the reamer is too large, and the cutting edges are not on the same circumference; excessive allowance for the reamed hole; uneven or too small allowance for the reamed hole, leading to unreamed local surfaces; excessive runout of the cutting part of the reamer, dull cutting edges, and rough surfaces; the cutting edge is too wide; poor chip removal during reaming; excessive wear of the reamer; the reamer is damaged, leaving burrs or chipping on the cutting edge; the cutting edge has built-up edge; due to material properties, it is not suitable for zero or negative rake angle reamers. 2) Solutions Lower the cutting speed; select cutting fluids based on the material being processed; appropriately reduce the main angle and correctly grind the cutting edge of the reamer; appropriately reduce the allowance for the reamed hole; improve the position accuracy and quality of the pre-drilled hole or increase the allowance for the reamed hole; select qualified reamers; grind the width of the cutting edge; reduce the number of teeth on the reamer based on specific conditions, increase the chip space, or use reamers with cutting edge inclination to facilitate chip removal; regularly replace reamers, and grind away the grinding area; during grinding, use protective measures to avoid damage; for damaged reamers, use a fine oil stone to repair the damaged reamer or replace it; grind to meet standards, using reamers with a rake angle of 5°-10°. 6. Low tool life of the reamer 1) Causes Inappropriate material for the reamer; burning during grinding; inappropriate selection of cutting fluid, leading to poor flow of cutting fluid, and high roughness value of the cutting surface and the surface after grinding the cutting edge. 2) Solutions Select reamer materials based on the processed material, using carbide or coated reamers; strictly control the grinding cutting amount to avoid burning; regularly select cutting fluids based on the processed material; frequently clear chips from the chip space, using cutting fluids with sufficient pressure, and achieve requirements through fine grinding or polishing. 7. Excessive deviation in the position accuracy of the reamed hole 1) Causes Wear of the guide sleeve; the bottom end of the guide sleeve is too far from the workpiece; the guide sleeve is short, has poor precision, and the spindle bearings are loose. 2) Solutions Regularly replace the guide sleeve; lengthen the guide sleeve to improve the fit precision between the guide sleeve and the reamer; timely repair the machine and adjust the spindle bearing gap. 8. Chipping of the reamer teeth 1) Causes Excessive allowance for the reamed hole; the hardness of the workpiece material is too high; excessive runout of the cutting edge, uneven cutting load; the main angle of the reamer is too small, increasing the cutting width; when reaming deep or blind holes, excessive chips are generated and not cleared in time, and the teeth are already cracked during grinding. 2) Solutions Modify the pre-processed hole diameter; reduce the material hardness or switch to negative rake angle reamers or carbide reamers; control runout within acceptable limits; increase the main angle; pay attention to timely chip removal or use reamers with cutting edge inclination; ensure grinding quality. 9. Breakage of the reamer shank 1) Causes Excessive allowance for the reamed hole; inappropriate distribution of rough and fine reaming allowances and cutting amounts when reaming conical holes; small chip space in the reamer teeth, leading to chip blockage. 2) Solutions Modify the pre-processed hole diameter; adjust the allowance distribution and choose cutting amounts reasonably; reduce the number of teeth on the reamer, increase chip space, or grind away one tooth of the cutting edge. 10. The centerline of the hole is not straight after reaming 1) Causes The drilling before reaming is misaligned, especially when the hole diameter is small, due to the poor rigidity of the reamer, which cannot correct the original curvature; the main angle of the reamer is too large; poor guidance causes the reamer to easily deviate during reaming; excessive taper of the cutting part; displacement of the reamer at the gap in the interrupted hole; when hand reaming, excessive force in one direction causes the reamer to tilt to one side, damaging the verticality of the reamed hole. 2) Solutions Increase reaming or boring processes to correct the hole; reduce the main angle; adjust to an appropriate reamer; replace with a reamer that has guiding parts or lengthen the cutting part; pay attention to correct operation. (Adapted from Metal Processing)

                                                        Common Problems and Solutions in Deep Hole Machining

During the deep hole machining process, issues such as the size precision, surface quality of the workpiece, and tool life often arise. How to reduce or even avoid these problems is a pressing issue we need to address.

1. Increased hole diameter, large error

1) Causes

The design value of the reamer's outer diameter is too large or the cutting edge has burrs; cutting speed is too high; improper feed rate or excessive machining allowance; the main angle of the reamer is too large; the reamer is bent; chips adhere to the cutting edge; the runout during grinding exceeds the limit; inappropriate selection of cutting fluid; oil stains on the taper shank surface are not cleaned before installing the reamer, or the taper surface has bumps; the flat tail of the taper shank is misaligned when installed in the machine spindle, causing conical interference; spindle bending or spindle bearings are too loose or damaged; the reamer is not flexible; misalignment with the workpiece and uneven force applied by both hands when hand reaming, causing the reamer to wobble.

2) Solutions

Appropriately reduce the outer diameter of the reamer based on specific conditions; lower the cutting speed; adjust the feed rate or reduce the machining allowance; appropriately reduce the main angle; straighten or scrap bent reamers that cannot be used; carefully grind to meet standards with an oilstone; control runout within acceptable limits; choose cutting fluids with good cooling performance; before installing the reamer, clean the oil stains from the reamer's taper shank and the internal taper hole of the machine spindle, and polish any bumps on the taper surface with an oilstone; grind the flat tail of the reamer; adjust or replace the spindle bearings; readjust the floating chuck and check coaxiality; pay attention to correct operation.

2. Decreased hole diameter

1) Causes

The design value of the reamer's outer diameter is too small; cutting speed is too low; feed rate is too high; the main angle of the reamer is too small; inappropriate selection of cutting fluid; during grinding, the worn part of the reamer is not ground away, causing elastic recovery that reduces the hole diameter; when reaming steel parts, excessive allowance or dull reamer can lead to elastic recovery, resulting in reduced hole diameter and non-circular inner holes, making the hole diameter unqualified.

2) Solutions

Replace the outer diameter of the reamer; appropriately increase the cutting speed; appropriately reduce the feed rate; appropriately increase the main angle; choose cutting fluids with good lubrication properties; regularly interchange reamers and correctly grind the cutting part of the reamer; when designing the reamer size, consider the above factors or take values based on actual conditions; conduct experimental cutting, take appropriate allowances, and sharpen the reamer.

3. Non-circular inner holes

1) Causes

The reamer is too long, lacks rigidity, and vibrates during reaming; the main angle of the reamer is too small; the cutting edge is too narrow; the reaming allowance is off; the inner hole surface has notches or intersecting holes; the hole surface has sand holes or air holes; spindle bearings are loose, there is no guide sleeve, or the gap between the reamer and the guide sleeve is too large, and due to the tight clamping of thin-walled workpieces, deformation occurs after removal.

2) Solutions

For reamers with insufficient rigidity, use reamers with unequal tooth pitch, and install the reamer using a rigid connection, increasing the main angle; select qualified reamers and control the hole position tolerance in the pre-processing stage; use reamers with unequal tooth pitch and longer, more precise guide sleeves; select qualified blanks; when reaming more precise holes with equal tooth pitch reamers, adjust the machine spindle's clearance, and the guide sleeve's fit gap should be high or use appropriate clamping methods to reduce clamping force.

4. Obvious edges on the inner surface of the hole

1) Causes

Excessive reaming allowance; the back angle of the cutting part of the reamer is too large; the cutting edge is too wide; the workpiece surface has air holes, sand holes, and excessive spindle runout.

2) Solutions

Reduce the reaming allowance; reduce the back angle of the cutting part; grind the width of the cutting edge; select qualified blanks; adjust the machine spindle.

5. High roughness value of the inner hole surface

1) Causes

Cutting speed is too high; inappropriate selection of cutting fluid; the main angle of the reamer is too large, and the cutting edge is not on the same circumference; excessive reaming allowance; uneven or too small reaming allowance, with some surfaces not reamed; excessive runout of the cutting part of the reamer, dull cutting edge, rough surface; cutting edge is too wide; poor chip removal during reaming; excessive wear of the reamer; the reamer is damaged, leaving burrs or chipping on the cutting edge; the cutting edge has chip buildup; due to material properties, it is not suitable for zero or negative rake angle reamers.

2) Solutions

Lower the cutting speed; select cutting fluid based on the material being processed; appropriately reduce the main angle, and correctly grind the cutting edge of the reamer; appropriately reduce the reaming allowance; improve the position accuracy and quality of the pre-drilled hole or increase the reaming allowance; select qualified reamers; grind the width of the cutting edge; reduce the number of teeth on the reamer based on specific conditions, increase the chip space, or use reamers with cutting edge inclination to facilitate chip removal; regularly replace reamers, and grind away the grinding area; during grinding, use protective measures to avoid damage; for damaged reamers, use a fine oilstone to repair or replace the reamer; grind to meet standards, using reamers with a rake angle of 5°-10°.

6. Low tool life of the reamer

1) Causes

Inappropriate reamer material; burning during grinding of the reamer; inappropriate selection of cutting fluid, leading to poor flow of cutting fluid, and high roughness value of the surface after grinding the cutting edge.

2) Solutions

Select reamer materials based on the processed materials, using carbide or coated reamers; strictly control the grinding cutting amount to avoid burning; frequently select cutting fluids correctly based on the processed materials; regularly clear chips from the chip space, using cutting fluid with sufficient pressure, and achieve requirements through fine grinding or polishing.

7. Position accuracy of the reamed hole exceeds limits

1) Causes

Wear of the guide sleeve; the bottom end of the guide sleeve is too far from the workpiece; the guide sleeve is short, has poor precision, and the spindle bearings are loose.

2) Solutions

Regularly replace the guide sleeve; extend the guide sleeve to improve the matching accuracy of the gap between the guide sleeve and the reamer; timely maintain the machine tool and adjust the spindle bearing gap.

8. Chipping of the reamer teeth

1) Causes

Excessive reaming allowance; the hardness of the workpiece material is too high; excessive cutting edge runout, uneven cutting load; the main angle of the reamer is too small, increasing the cutting width; when reaming deep or blind holes, too many chips are generated and not cleared in time, and the teeth have cracked during grinding.

2) Solutions

Modify the pre-processed hole diameter; reduce material hardness or use a negative rake angle reamer or carbide reamer; control the runout within acceptable limits; increase the main angle; pay attention to timely chip removal or use a reamer with a cutting edge inclination angle; pay attention to grinding quality.

9. Breakage of the reamer shank

1) Causes

Excessive reaming allowance; when reaming tapered holes, the allocation of rough and fine reaming allowances and the selection of cutting amounts are inappropriate; the chip space of the reamer teeth is small, causing chip blockage.

2) Solutions

Modify the pre-processed hole diameter; adjust the allowance distribution and reasonably select the cutting amount; reduce the number of reamer teeth, increase the chip space, or grind away one tooth of the reamer.

10. The centerline of the hole after reaming is not straight

1) Causes

The drilling before reaming is skewed, especially when the hole diameter is small, due to the poor rigidity of the reamer, it cannot correct the original curvature; the main angle of the reamer is too large; poor guidance causes the reamer to easily deviate during reaming; the cutting part has excessive taper; the reamer shifts at the gap in the middle of the intermittent hole; when hand reaming, excessive force is applied in one direction, forcing the reamer to tilt to one end, damaging the verticality of the reamed hole.

2) Solutions

Increase the reaming or boring process to correct the hole; reduce the main angle; adjust the appropriate reamer; replace with a reamer that has a guiding part or extend the cutting part of the reamer; pay attention to correct operation. (Adapted from Metal Processing)

TAG:


RELATED INFORMATION

ADD

Gengguantun Industrial Development Zone, Qingxian County, Hebei Province, China

WeChat applet

WeChat applet

Business License