【Summary】After bending, aluminum plates may crack easily, or they may burst after anodizing. Many sheet metal processing companies are confused by this. So how can we prevent cracking? Several main reasons and precautions for cracking after bending aluminum plates: 1. Hardness of the aluminum plate. If the hardness of the aluminum plate is too high, it can crack easily. Therefore, it is necessary to choose the right aluminum material, mainly looking at the aluminum material's brand and condition. Generally, series 1, 3, and 5 are commonly used; series 6 and 7 have too high hardness and should be annealed to O state before bending. Additionally, the quality of the aluminum plate matters; imported aluminum plates of the same type are less likely to crack than domestic ones, but the material cost is also significantly higher. 2. Thickness of the aluminum plate. Thicker aluminum plates are difficult to bend. It is advisable to use thinner aluminum plates whenever possible. 3. Size of the bending R angle. The larger the bending R angle, the higher the success rate, so it is best to increase the bending R angle as much as possible. 4. Direction of the aluminum plate's grain. The bending direction should be perpendicular to the grain direction of the aluminum plate, not parallel. 5. For aluminum plate parts that require brushing, it is best to bend them before brushing if the process allows, otherwise, it will increase the probability of cracking during bending. If these aspects are well addressed, the issue of cracking during the bending of aluminum plates can be effectively resolved.

                                   Precautions for processing aluminum plates in sheet metal processing

Aluminum plates may crack easily after bending, or they may burst after anodizing. Many sheet metal processing companies are confused by this, so how can we prevent cracking?

Several main reasons and precautions for cracking of aluminum plates after bending:

The hardness of the aluminum plate.

If the hardness of the aluminum plate is too high, it can crack easily. Therefore, it is necessary to choose the right aluminum material, mainly looking at the aluminum material brand and condition. Generally, series 1, 3, and 5 are commonly used; series 6 and 7 have too high hardness and need to be annealed to O state before bending. Also, the quality of the aluminum plate matters; imported aluminum plates of the same type are less likely to crack than domestic ones, but the material cost is also significantly higher.

The thickness of the aluminum plate.

Too thick aluminum plates are difficult to bend, which is understandable; it is best to use thinner aluminum plates.

The size of the bending R angle.

The larger the bending R angle, the higher the success rate, so try to increase the bending R angle as much as possible.

The grain direction of the aluminum plate.

The bending direction must be perpendicular to the grain direction of the aluminum plate, not parallel.

For aluminum plate parts that require brushing, it is best to bend them before brushing if the process allows, otherwise it will increase the probability of cracking during bending.

If the above aspects are handled well, the issue of cracking during the bending of aluminum plates will be better addressed.