Machining Technology Requirements


Release time:

2021-03-27

【Summary】Tolerance Requirements 1. Unmarked shape tolerances should comply with GB1184-80 requirements. 2. Unmarked length dimensions allow a deviation of ±0.5mm. 3. The tolerance zone of castings is symmetrical to the basic dimensions of the blank casting. Part Edges 1. Unmarked corner radius R5. 2. Unmarked chamfers are all 2×45°. 3. Sharp angles/points/edges should be rounded. Assembly Requirements 1. All sealing components must be soaked in oil before assembly. 2. For the assembly of rolling bearings, heating with machine oil is allowed for hot installation, and the oil temperature must not exceed 100°C. 3. After gear assembly, the contact spots on the tooth surface and the side clearance should comply with GB10095 and GB11365 regulations. 4. When assembling the hydraulic system, sealing fillers or sealants are allowed, but should be prevented from entering the system. 5. Parts and components (including purchased and outsourced parts) entering assembly must have a certificate of conformity from the inspection department. 6. Parts must be cleaned and washed before assembly, free of burrs, flash, oxide scale, rust, chips, oil stains, coloring agents, and dust. 7. Before assembly, the main mating dimensions of parts should be rechecked, especially the interference fit dimensions and related precision. 8. During assembly, parts must not be knocked, bumped, scratched, or corroded. 9. When tightening screws, bolts, and nuts, striking or using inappropriate tools and wrenches is strictly prohibited. After tightening, the screw slots and fasteners requiring specified torque must use a torque wrench and be tightened according to the specified torque. 10. When fastening the same part with multiple screws (bolts), each screw (bolt) must be tightened in a cross, symmetrical, gradual, and uniform manner. 11. When assembling conical pins, a color check should be performed with the holes, and the contact rate should not be less than 60% of the fitting length, and should be evenly distributed. 12. The flat key should have uniform contact on both sides of the keyway on the shaft, and there should be no gaps on the mating surface. 13. The number of tooth surfaces in contact during spline assembly should not be less than 2/3, and the contact rate in the length and height direction of the key teeth should not be less than 50%. 14. After the assembly of sliding fit flat keys (or splines), the matching parts should move freely without uneven tightness. 15. Excess adhesive should be removed after bonding. 16. The outer ring of the bearing must not be stuck in the open bearing seat and bearing cover's semicircular hole. 17. The outer ring of the bearing should have good contact with the open bearing seat and bearing cover's semicircular hole. When checked with color, it should have uniform contact within the range symmetrical to the centerline of 120° with the bearing seat and 90° with the bearing cover. When checked with a feeler gauge within the above range, a 0.03mm feeler gauge should not be inserted into 1/3 of the outer ring width. 18. After the outer ring of the bearing is assembled, it should have uniform contact with the end face of the positioning end bearing cover. 19. After the rolling bearing is installed, it should rotate flexibly and smoothly by hand. 20. The mating surface of the upper and lower bearing shells should be closely fitted, and should not allow a 0.05mm feeler gauge to enter. 21. When fixing the bearing shell with positioning pins, drilling and fitting pins should be done while ensuring that the bearing surface and end face are flush with the corresponding bearing hole's opening and end face. The pins should not be loose after being driven in. 22. The bearing body of the spherical bearing should have uniform contact with the bearing seat, and should be checked with the color method, with contact not less than 70%. 23. Alloy bearing liners with a yellow surface should not be used. There should be no core separation within the specified contact angle, and the area of core separation outside the contact angle should not exceed 10% of the total area of the non-contact zone. 24. The reference end face of the gear (worm gear) should fit with the shaft shoulder (or positioning sleeve end face), and should not allow a 0.05mm feeler gauge to enter. The verticality requirement of the gear reference end face to the axis should also be ensured. 25. The mating surface of the gearbox and cover should have good contact. 26. Before assembly, strictly check and remove sharp angles, burrs, and foreign objects left over from part processing. Ensure that sealing components are not scratched during installation. Casting Requirements 1. The surface of the casting must not have cold shuts, cracks, shrinkage cavities, penetrating defects, or serious defects such as undercasting and mechanical damage. 2. The casting should be cleaned and free of burrs and flash, and the non-machined surface's pouring risers should be cleaned to be flush with the casting surface. 3. The cast letters and marks on the non-machined surface of the casting should be clear and legible, and the position and font should meet the drawing requirements. 4. The roughness of the non-machined surface of the casting, sand casting R, should not exceed 50μm. 5. The casting should be free of pouring risers, flash, etc. The residual amount of pouring risers on the non-machined surface should be leveled and polished to meet surface quality requirements. 6. The molding sand, core sand, and core skeleton on the casting should be thoroughly cleaned. 7. For inclined parts of the casting, the size tolerance zone should be symmetrically configured along the inclined surface. 8. The molding sand, core sand, core skeleton, excess meat, and sand adhesion on the casting should be leveled and cleaned. 9. For incorrect shapes, protruding castings, etc., corrections should be made to achieve smooth transitions and ensure appearance quality. 10. The wrinkles on the non-machined surface of the casting should have a depth of less than 2mm, and the spacing should be greater than 100mm. 11. The non-machined surfaces of machine product castings must be shot peened or tumbled to meet the cleanliness requirement of Sa2 1/2 level. 12. The casting must undergo water toughness treatment. 13. The surface of the casting should be flat, and the pouring gates, burrs, and sand adhesion should be thoroughly cleaned. 14. The casting must not have casting defects such as cold shuts, cracks, or holes that are detrimental to use. Coating Requirements 1. All steel parts that require coating must have rust, oxide scale, grease, dust, dirt, salt, and contaminants removed from the surface before painting. 2. Before rust removal, the surface grease and dirt of the steel parts should be removed using organic solvents, alkaline solutions, emulsifiers, steam, etc. 3. The time interval between the surface to be coated after shot blasting or manual rust removal and the application of primer should not exceed 6 hours. 4. The surfaces of riveted parts that come into contact must be coated with a rust-proof paint of thickness 30-40μm before connection. Overlapping edges should be sealed with paint, putty, or adhesive. Damaged primer due to processing or welding should be repainted. Piping Requirements 1. Before assembly, all pipes should have burrs and sharp edges removed from the ends. Use compressed air or other methods to clear debris and floating rust from the inner walls of the pipes. 2. Before assembly, all steel pipes (including prefabricated pipelines) must undergo degreasing, acid cleaning, neutralization, water washing, and rust prevention treatment. 3. During assembly, parts fixed with threaded connections such as pipe clamps, supports, flanges, and joints should be tightened to prevent loosening. 4. The welded joints of prefabricated pipes must undergo pressure testing. 5. When replacing or transferring pipes, the pipe separation points must be sealed with tape or plastic tubes to prevent any debris from entering, and labeled. Repair Welding Requirements 1. Defects must be thoroughly removed before welding, and the bevel surface should be smooth and rounded without sharp corners. 2. Depending on the defect situation of the cast steel parts, defects in the welding area can be removed using methods such as gouging, grinding, carbon arc air gouging, cutting, or machining. 3. Dirt such as sand adhesion, oil, water, and rust within 20mm around the welding area and bevel must be thoroughly cleaned. 4. During the entire welding process, the preheating area of the cast steel parts must not be below 350°C. 5. If conditions permit, welding should be performed in a horizontal position as much as possible. 6. During repair welding, the welding rod should not swing excessively sideways. 7. When overlay welding on the surface of cast steel parts, the overlap between weld beads should not be less than 1/3 of the weld bead width. The weld metal should be full, and the welding surface should be free of burn marks, cracks, and obvious lumps. The appearance of the weld should be beautiful, without defects such as undercutting, slag inclusion, porosity, cracks, or spatter; the weld ripples should be uniform. Forging Requirements 1. The water inlet and riser of the ingot should have sufficient removal to ensure that the forging has no shrinkage cavities and serious deflections. 2. The forging should be shaped on a forging press with sufficient capacity to ensure that the internal structure of the forging is fully forged. 3. The forging must not have visible cracks, folds, or other appearance defects that affect use. Local defects can be removed, but the cleaning depth must not exceed 75% of the machining allowance, and defects on the non-machined surface of the forging should be cleaned and smoothly transitioned. 4. The forging must not have white spots, internal cracks, or residual shrinkage cavities. Machining Requirements 1. Parts should be inspected and accepted according to the process, and only after passing the inspection of the previous process can they proceed to the next process. 2. Processed parts must not have burrs. 3. Finished parts should not be placed directly on the ground; necessary support and protection measures should be taken. The machined surfaces must not have rust, and defects that affect performance, lifespan, or appearance such as bumps and scratches are not allowed. 4. The surface of parts that have been rolled and finished should not have peeling. 5. After the final heat treatment process, the surface of the parts should not have oxide scale. The machined mating surfaces and tooth surfaces should not have annealing. 6. The machined threaded surfaces must not have black skin, bumps, cross-threading, or burrs.

                                      Machining Technical Requirements   

General Technical Requirements
1. Remove the oxidation skin from the parts.
2. There should be no scratches, abrasions, or other surface defects on the machined surface of the parts.
3. Remove burrs and flash.
Heat Treatment Requirements
1. After quenching and tempering, HRC 50-55.
2. Parts undergo high-frequency quenching, tempering at 350-370℃, HRC 40-45.
3. Carburizing depth of 0.3mm.

4. Perform high-temperature aging treatment.

Tolerance Requirements
1. Unspecified shape tolerances should comply with GB1184-80.
2. Unspecified length dimensions allowed deviation ±0.5mm.
3. The tolerance zone of castings is symmetrical to the basic dimensions of the blank casting.
Part Edges and Corners
1. Unspecified corner radius R5.
2. Unspecified chamfers are all 2×45°.
3. Sharp angles/points/edges should be rounded.
Assembly Requirements
1. All sealing components must be soaked in oil before assembly.
2. Rolling bearings may be heated with oil for hot assembly, and the oil temperature must not exceed 100℃.
3. After gear assembly, the contact spots on the tooth surfaces and the side gaps should comply with GB10095 and GB11365.
4. When assembling the hydraulic system, sealing fillers or sealants may be used, but care should be taken to prevent them from entering the system.
5. Parts and components (including purchased and outsourced parts) entering assembly must have a certificate of conformity from the inspection department.
6. Parts must be cleaned and washed before assembly, free of burrs, flash, oxidation skin, rust, chips, oil stains, coloring agents, and dust.
7. Before assembly, the main mating dimensions of the parts should be rechecked, especially the interference fit dimensions and related precision.
8. During assembly, parts must not be knocked, bumped, scratched, or corroded.
9. When tightening screws, bolts, and nuts, it is strictly forbidden to strike or use inappropriate tools and wrenches. After tightening, the screw slots and fasteners that require specified torque must use a torque wrench and be tightened to the specified torque.
11. When fastening the same part with multiple screws (bolts), each screw (bolt) must be tightened in a cross, symmetrical, gradual, and uniform manner.
12. When assembling tapered pins, color checks should be performed with the holes, and the contact rate should not be less than 60% of the fitting length, and should be evenly distributed.
 
13. The flat key and the keyway on the shaft should contact evenly, and there should be no gaps on the mating surfaces.
 
14. The number of tooth surfaces in contact during spline assembly should not be less than 2/3, and the contact rate in the length and height direction of the key teeth should not be less than 50%.
15. After assembly of sliding fit flat keys (or splines), the matched parts should move freely, and there should be no uneven tightness.
16. Excess adhesive should be removed after bonding.
17. The outer ring of the bearing must not be stuck in the open bearing seat and bearing cover's semicircular hole.
18. The outer ring of the bearing should have good contact with the open bearing seat and bearing cover. When checked with color, it should have uniform contact within the range symmetrical to the centerline at 120° with the bearing seat and 90° with the bearing cover. When checked with a feeler gauge in the above range, a 0.03mm feeler gauge must not fit into 1/3 of the outer ring width.
19. After the outer ring of the bearing is assembled, it should contact evenly with the end face of the positioning end bearing cover.
20. After the rolling bearing is installed, it should rotate flexibly and smoothly by hand.
21. The joint surface of the upper and lower bearing shells should be closely fitted, and should not allow a 0.05mm feeler gauge to enter.
22. When fixing the bearing shell with positioning pins, drilling and fitting should be done while ensuring that the bearing mouth surface and end face are flush with the corresponding bearing hole's opening and end face. The pin must not loosen after being driven in.
23. The bearing body of the spherical bearing should contact evenly with the bearing seat. When checked with the color method, the contact should not be less than 70%.
24. Alloy bearing liners should not be used when the surface turns yellow. There should be no core separation within the specified contact angle, and the area of core separation outside the contact angle should not exceed 10% of the total area of the non-contact zone.
25. The reference end face of the gear (worm gear) should fit with the shaft shoulder (or positioning sleeve end face), and should not allow a 0.05mm feeler gauge to enter. The verticality requirement of the gear reference end face to the axis should also be ensured.
26. The joint surface of the gearbox and cover should have good contact.
27. Strictly check and remove sharp angles, burrs, and foreign objects left on parts during processing before assembly. Ensure that sealing components are not scratched during installation.
 
Casting Requirements
1. The surface of the casting shall not have cold shuts, cracks, shrinkage cavities, penetrating defects, or serious defects such as undercasting and mechanical damage.
2. The casting should be cleaned thoroughly, with no burrs or flash, and the non-machined surface of the pouring riser should be cleaned flush with the casting surface.
3. The cast letters and marks on the non-machined surface of the casting should be clear and legible, and the position and font should meet the requirements of the drawings.
4. The roughness of the non-machined surface of the casting, sand casting R, shall not exceed 50 μm.
5. The casting should remove pouring risers, flash, etc. The residual amount of pouring risers on the non-machined surface should be leveled and polished to meet surface quality requirements.
6. The molding sand, core sand, and core skeleton on the casting should be cleaned thoroughly.
7. For inclined parts of the casting, the dimensional tolerance band should be symmetrically configured along the inclined surface.
8. The molding sand, core sand, core skeleton, excess material, and sand adhesion on the casting should be leveled and cleaned.
9. Incorrect shapes, offset castings, etc. should be corrected to achieve a smooth transition, ensuring appearance quality.
10. The wrinkles on the non-machined surface of the casting should have a depth of less than 2mm, and the spacing should be greater than 100mm.
11. The non-machined surfaces of machine product castings must undergo shot peening or tumbling treatment to meet the cleanliness requirement of Sa2 1/2 level.
12. The casting must undergo water toughening treatment.
13. The surface of the casting should be flat, and the pouring gates, burrs, sand adhesion, etc. should be cleaned thoroughly.
14. The casting is not allowed to have casting defects such as cold shuts, cracks, or holes that are detrimental to use.
Coating Requirements
1. All steel parts that require coating must be free of rust, scale, grease, dust, dirt, salt, and other contaminants before painting.
2. Before rust removal, use organic solvents, alkaline solutions, emulsifiers, steam, etc. to remove grease and dirt from the surface of the steel parts.
3. The time interval between shot peening or manual rust removal and applying the primer should not exceed 6 hours.
4. The surfaces of riveted parts that come into contact with each other must be coated with rust-proof paint with a thickness of 30 to 40 μm before connection. The overlapping edges should be sealed with paint, putty, or adhesive. Any damaged primer due to processing or welding must be repainted.
 
Piping Requirements
1. Before assembly, all pipes should have burrs and sharp edges removed from the ends. Use compressed air or other methods to clear any debris and rust from the inner walls of the pipes.
2. Before assembly, all steel pipes (including prefabricated pipelines) must undergo degreasing, acid cleaning, neutralization, water washing, and rust-proof treatment.
3. During assembly, parts fixed with threaded connections such as pipe clamps, supports, flanges, and joints should be tightened to prevent loosening.
4. The welded joints of prefabricated pipes must undergo pressure testing.
5. When replacing or transporting pipes, the separation points of the pipelines must be sealed with tape or plastic tubes to prevent any debris from entering, and labeled.
Repair Welding Requirements
1. Defects must be completely removed before welding, and the bevel surface should be smooth and rounded, with no sharp corners.
2. Depending on the defect situation of the cast steel parts, defects in the welding area can be removed using methods such as gouging, grinding, carbon arc air gouging, cutting, or machining.
3. Dirt such as sand adhesion, oil, water, and rust within 20mm around the welding area and bevel must be thoroughly cleaned.
4. During the entire welding process, the preheating temperature of the cast steel parts must not be lower than 350°C.
5. If conditions permit, welding should be done in a horizontal position as much as possible.
6. During repair welding, the welding rod should not swing too much laterally.
7. When overlay welding on the surface of cast steel parts, the overlap between weld beads should not be less than 1/3 of the width of the weld bead. The weld metal should be full, with no burn-through, cracks, or obvious lumps. The appearance of the weld should be beautiful, with no defects such as undercutting, slag inclusion, porosity, cracks, or spatter; the weld ripples should be uniform.
Forging Requirements
1. The water inlet and riser of the ingot should have sufficient cutting amount to ensure that the forging has no shrinkage cavities and serious deflections.
2. The forging should be shaped on a forging press with sufficient capacity to ensure that the internal structure of the forging is fully forged.
3. The forging is not allowed to have visible cracks, folds, or other appearance defects that affect use. Local defects can be removed, but the cleaning depth must not exceed 75% of the machining allowance, and defects on the non-machined surface of the forging should be cleaned and smoothly transitioned.
4. The forging is not allowed to have white spots, internal cracks, or residual shrinkage cavities.
Machining Requirements
1. Parts should be inspected and accepted according to the process, and only after passing the inspection of the previous process can they proceed to the next process.
2. Processed parts are not allowed to have burrs.
3. Finished parts should not be placed directly on the ground; necessary support and protection measures should be taken. The machined surfaces should not have rust, and defects such as impacts, scratches that affect performance, lifespan, or appearance.
4. The surface of the rolled finish should not have any peeling after rolling.
5. The surface of parts after the final heat treatment should not have any oxidation scale. The machined mating surfaces and tooth surfaces should not have any annealing.
6. The machined threaded surfaces are not allowed to have defects such as black scale, bumps, miscuts, and burrs.

TAG:


RELATED INFORMATION

ADD

Gengguantun Industrial Development Zone, Qingxian County, Hebei Province, China

WeChat applet

WeChat applet

Business License