Several Methods to Control Chip Formation in Turning Processing


Release time:

2021-05-21

【Summary】In the machining process, the continuous generation of strip chips can not only scratch the surface of the workpiece and damage the cutting edge but can also pose a serious safety risk to the operator. Therefore, implementing necessary process measures to control chip formation and breaking is a critical issue in the machining industry. Chips are the result of deformation in the chip layer, and altering cutting conditions is an effective way to change chip types and achieve chip breaking. Key factors influencing cutting conditions include the material of the workpiece, the geometry of the cutting tool, and the volume of chips produced. Chips must meet several essential criteria: they should not wrap around the tool, workpiece, or adjacent equipment; they must not splatter to ensure the safety of operators and observers; during finishing, chips should not scratch the machined surface of the workpiece, affecting its quality; the tool's durability must be maintained to prevent premature wear and breakage; chips should not obstruct the flow of cutting fluid; and they should not damage the machine tool's guide rails or other components. 1. Classification of Chip Shapes Different degrees of plastic deformation can lead to various types of chips, as illustrated in Figure 1. When machining plastic materials, strip chips, segment chips, or granular chips are typically produced, while brittle materials generally yield fragmented chips. 1. Strip Chips: These are continuous chips with a smooth bottom surface and a fluffy back, as shown in Figure 1-1a. They are easily produced when using tools with a larger rake angle at higher cutting speeds on plastic metals. Strip chips result from insufficient deformation of the cutting layer. Although the cutting process is stable and the workpiece surface roughness is low, strip chips are difficult to break, often leading to entanglement and roughing of the workpiece, which cannot be overlooked. 2. Segment Chips: Characterized by a smooth bottom and deep cracks on the back, segment chips (Figure 1-1b) are produced when using tools with a reduced rake angle at lower cutting speeds on plastic materials. They result from more significant deformation of the chip layer, reaching shear fracture levels, leading to unstable cutting work and increased surface roughness. 3. Granular Chips: These uniform, granular chips (Figure 1-1c) are produced when using small rake angle tools at very low cutting speeds on plastic metals. They result from sufficient deformation of the cutting layer, leading to shear failure and breaking along their thickness, causing unstable cutting work and increased surface roughness. 4. Fragmented Chips: Irregular, fine granular chips (Figure 1-1d) are formed when cutting brittle materials, where the cutting layer fractures suddenly after elastic deformation without undergoing plastic deformation. This results in unstable cutting work and significant impact forces on the cutting edge, leading to a rough machined surface. The type of chips produced varies with the workpiece material and cutting conditions. Thus, observing chip morphology during machining can help assess the suitability of chip conditions, and altering cutting conditions can change chip morphology to favor production. 2. Principle of Chip Breaking In metal cutting, the ease of chip breaking is directly related to chip deformation. Therefore, understanding the principles of chip breaking requires studying the laws of chip deformation. Chips formed during cutting undergo significant plastic deformation, increasing their hardness while reducing plasticity and toughness, a phenomenon known as cold work hardening. After this process, chips become hard and brittle, making them prone to breaking under alternating bending or impact loads. The greater the plastic deformation, the more pronounced the hard and brittle characteristics, facilitating breaking. When cutting materials that are difficult to break, efforts should be made to increase chip deformation to reduce plasticity and toughness, aiding in chip breaking. Chip deformation consists of two parts: The first part is the basic deformation occurring during cutting, which can be measured using a flat front tool. The main factors affecting this basic deformation are the rake angle, negative chamfer, and cutting speed. A smaller rake angle, wider negative chamfer, and lower cutting speed result in greater chip deformation, which is beneficial for breaking chips. Thus, reducing the rake angle, widening the negative chamfer, and lowering the cutting speed are effective measures to promote chip breaking. The second part is the additional deformation experienced by chips during flow and curling, referred to as additional deformation. In most cases, basic deformation alone is insufficient for chip breaking; additional deformation is necessary to achieve hardening and breaking. The simplest way to induce additional deformation is to create a specific chip breaking groove on the front tool surface, forcing chips to flow into the groove and undergo further curling deformation. This additional deformation leads to further hardening and brittleness, making chips easier to break upon contact with the workpiece or back tool surface. 3. Chip Breaking Methods The fundamental reason for chip breaking lies in the deformation and stress during chip formation. Chips will break when they are in an unstable deformation state or when the stress reaches their strength limit, typically breaking after curling. Common chip breaking methods include selecting appropriate tool geometry angles, adjusting cutting volume, and grinding chip breaking grooves. 1. Reduce the rake angle and increase the main inclination angle: The rake angle and main inclination angle significantly impact chip breaking. Reducing the rake angle increases chip deformation, facilitating breaking. However, this also increases cutting force, which can limit cutting volume and potentially damage the tool or cause stalling. Therefore, reducing the rake angle alone is generally not sufficient for chip breaking. Increasing the main inclination angle can enhance cutting thickness, making it easier to break chips. For instance, under the same conditions, a 90° tool is more effective for breaking chips than a 45° tool. Additionally, increasing the main inclination angle helps reduce vibrations during machining, making it an effective chip breaking method. 2. Reduce cutting speed and increase feed rate: Adjusting cutting volume is another method for chip breaking. Increasing cutting speed softens the metal at the base of the chips, leading to insufficient deformation and hindering chip breaking. Conversely, reducing cutting speed facilitates chip breaking. Therefore, during turning, lowering spindle speed and cutting speed can aid in chip breaking. Increasing feed rate can also enhance cutting thickness, making it easier to break chips. This is a commonly used method in machining, but it should be noted that increasing feed rate can significantly raise the surface roughness of the workpiece. 3. Establish chip breaking grooves: Chip breaking grooves are grooves created on the front tool surface. The shape, width, and angle of these grooves all influence chip breaking. 1) Shape of the chip breaking groove: Common shapes include zigzag, straight arc, and full arc, as shown in Figure 2. When cutting carbon steel, alloy steel, and tool steel, zigzag or straight arc grooves can be used; for high plasticity materials like pure copper and stainless steel, full arc grooves are preferable. 2) Width of the chip breaking groove: The width significantly affects chip breaking. Generally, a smaller groove width results in a smaller curling radius, increasing the bending stress on the chips and making them easier to break. Therefore, narrower chip breaking grooves are beneficial. However, the groove width must be considered in relation to feed rate and cutting depth (αp). If the groove width is appropriately matched to the feed rate, a C-shaped chip can form. If the groove is too narrow, it may cause chip blockage, increasing the load on the cutting tool and potentially damaging the cutting edge; if too wide, the curling radius may be excessive, leading to insufficient deformation and difficulty in breaking, often resulting in continuous strip chips that do not flow through the groove. The groove width should also be suitable for the cutting depth; otherwise, if too narrow, the chips will appear wide and not curl easily, leading to strip chips that do not flow through the groove. If too wide, the chips will appear narrow and flow freely, but will not undergo sufficient deformation, also failing to break. To achieve satisfactory chip breaking results, the appropriate width of the chip breaking groove should be selected based on specific machining conditions. For softer workpiece materials, narrower grooves are recommended, while for harder materials, wider grooves should be chosen.

                                    Several methods to control chip breaking in turning processing

During the process, when continuous strip chips are produced, they not only easily scratch the surface of the workpiece and damage the cutting edge, but in severe cases, they can also threaten the safety of the operator. Therefore, taking necessary process measures to control chip shape and breaking has always been an extremely important process issue in the machining industry.

Since chips are the product of the deformation of the chip layer, changing the cutting processing conditions is an effective way to change the type of chips and achieve chip breaking. The main factors affecting the chip processing conditions include workpiece material, tool geometry angles, and chip volume.
Generally, chips need to meet the following basic conditions: chips must not wrap around the tool, workpiece, and adjacent tools or equipment; chips must not splash to ensure the safety of operators and observers; during finishing, chips must not scratch the already processed surface of the workpiece, affecting the quality of the processed surface; ensure the predetermined durability of the tool, preventing premature wear and striving to avoid breakage; when chips flow out, they should not obstruct the spraying of cutting fluid; chips should not scratch the machine tool guide rails or other components.
I. Classification of Chip Shapes
Due to different degrees of plastic deformation, different types of chips may be produced, as shown in Figure 1. When processing plastic materials, strip chips, segment chips, or granular chips are mainly formed; when processing brittle materials, fragmented chips are generally formed.
Image
1. Strip Chips: Strip chips are continuous, with a smooth bottom surface and a fluffy back surface, as shown in Figure 1-1a. When using tools with a larger rake angle and processing plastic metal materials at a higher cutting speed, this type of chip is easily produced. It is a product of insufficient deformation of the cutting layer. When strip chips are produced, the cutting process is stable, and the surface roughness of the workpiece is relatively small, but the chips are not easy to break, often causing entanglement, roughening the workpiece, and even affecting operation, so the issue of chip breaking cannot be ignored.
 
2. Segment Chips: Segment chips have a smooth bottom surface and obvious cracks on the back, with deeper cracks, as shown in Figure 1-1b. When using tools with a reduced rake angle and processing plastic materials at a lower cutting speed, this type of chip is easily produced. It is a product of more sufficient deformation of the chip layer, having reached the level of shear fracture. When segment chips are produced, the chip work is unstable, and the surface roughness of the workpiece is larger.
3. Granular Chips: Granular chips are uniform, granular chips, as shown in Figure 1-1c. When using small rake angle tools and processing plastic metal materials at very low cutting speeds, this type of chip is easily produced. It is a product of sufficient deformation of the cutting layer, having reached the level of material shear failure, causing the chips to break along their thickness. When granular chips are produced, the cutting work is unstable, and the surface roughness of the workpiece is larger.
4. Fragmented Chips: Fragmented chips are irregular, fine granular chips, as shown in Figure 1-1d. They are formed when cutting brittle materials, where the cutting layer, after elastic deformation, almost does not go through the plastic deformation stage and suddenly fractures. When fragmented chips are formed, the cutting work is unstable, and the cutting edge experiences significant impact forces, resulting in a rough and uneven processed surface.
From the above, it can be seen that the type of chips varies with the workpiece material and cutting conditions. Therefore, during the processing, one can judge whether the chip conditions are appropriate by observing the chip shapes, and one can also change the chip shapes by altering the cutting conditions to transform them in a direction favorable to production.
II. Principles of Chip Breaking
In the metal cutting process, whether chips are easy to break is directly related to the deformation of the chips. Therefore, studying the principles of chip breaking must start from studying the laws of chip deformation.
The chips formed during the cutting process undergo significant plastic deformation, which increases their hardness while significantly reducing their plasticity and toughness. This phenomenon is called cold work hardening. After cold work hardening, the chips become hard and brittle, making them prone to breaking when subjected to alternating bending or impact loads. The greater the plastic deformation the chips undergo, the more pronounced the hard and brittle phenomenon becomes, and the easier they break. When cutting difficult-to-break materials with high strength, high plasticity, and high toughness, efforts should be made to increase the deformation of the chips to reduce their plasticity and toughness, facilitating the goal of chip breaking.
The deformation of chips can consist of two parts:
The first part is the deformation formed during the cutting process, which we call basic deformation. The chip deformation measured when using a flat front tool for free cutting is close to the value of basic deformation. The main factors affecting basic deformation are the tool's rake angle, negative chamfer, and cutting speed. The smaller the rake angle, the wider the negative chamfer, and the lower the cutting speed, the greater the deformation of the chips, which is more favorable for chip breaking. Therefore, reducing the rake angle, widening the negative chamfer, and lowering the cutting speed can be measures to promote chip breaking.
The second part is the deformation the chips undergo during flow and curling, which we call additional deformation. In most cases, the basic deformation during the cutting process alone is not sufficient to break the chips; additional deformation must be added to achieve hardening and breaking. The simplest way to force the chips to undergo additional deformation is to grind (or press) a certain shape of chip breaking groove on the front tool surface, forcing the chips to flow into the chip breaking groove and then curl and deform. After the chips undergo additional curling deformation, they further harden and become brittle, making them easy to break when they collide with the workpiece or the back tool surface.
 
III. Methods of Chip Breaking
The fundamental reason for chips breaking or not breaking lies in the deformation and stress during the chip formation process. When the chips are in an unstable deformation state or the stress on the chips reaches their strength limit, they will break, and typically, chips break after curling.
Reasonably selecting tool geometry angles, cutting volume, and grinding chip breaking grooves are common methods for chip breaking.
1. Reduce the front angle and increase the main relief angle: The front angle and main relief angle are the tool geometric angles that have a significant impact on chip breaking. Reducing the front angle intensifies chip deformation, making it easier to break chips. Since reducing the front angle increases cutting force, it limits the increase in cutting amount, and in severe cases, it can damage the tool or even cause "stalling". Generally, simply reducing the front angle is not used for chip breaking. Increasing the main relief angle can increase the cutting thickness, making it easier to break chips. For example, under the same conditions, a 90° tool is easier to break chips than a 45° tool. Additionally, increasing the main relief angle helps reduce vibrations during processing. Therefore, increasing the main relief angle is an effective method for chip breaking.
2. Reduce cutting speed and increase feed rate: Changing the cutting amount is another measure for chip breaking. Increasing the cutting speed softens the underlying metal of the chips and leads to insufficient chip deformation, which is not conducive to chip breaking; reducing the cutting speed, on the other hand, makes it easier to break chips. Therefore, during turning, chip breaking can be achieved by lowering the spindle speed and reducing the cutting speed. Increasing the feed rate can increase the cutting thickness, making it easier to break chips. This is a commonly used method for chip breaking in processing, but it should be noted that as the feed rate increases, the surface roughness of the workpiece will significantly increase.
3. Create chip breaking grooves: Chip breaking grooves refer to the grooves made on the front cutting face of the tool. The shape, width, and angle of the chip breaking groove are all factors that affect chip breaking.
1) Shape of the chip breaking groove
Common chip breaking grooves include three types: zigzag, straight arc, and full arc, as shown in Figure 2.
Image
When cutting carbon steel, alloy steel, and tool steel, zigzag, straight arc, and chip breaking grooves can be selected; when cutting high plasticity materials such as pure copper and stainless steel workpieces, full arc chip breaking grooves can be selected.
2) Width of the chip breaking groove
The width of the chip breaking groove greatly affects chip breaking. In general, a smaller groove width results in a smaller curling radius of the chips, which increases the bending stress on the chips, making them easier to break. Therefore, adopting a narrower chip breaking groove width is advantageous for chip breaking. However, the width of the chip breaking groove must be considered in conjunction with the feed rate and cutting depth (αp).
If the width of the chip breaking groove is basically suitable for the feed rate, a C-shaped chip can be formed. If the curling groove is too narrow, it is easy to cause chip blockage, which increases the load on the cutting tool and may even damage the cutting edge; if the curling groove is too wide, the curling radius of the chips is too large, leading to insufficient deformation and difficulty in breaking, often resulting in continuous strip chips that do not flow through the bottom of the groove.
The width of the chip breaking groove should also be appropriate for the cutting depth; otherwise, if the groove is too narrow, the chips appear wide and are not easy to curl in the groove, often resulting in chips that do not flow through the bottom of the groove, forming strip chips. When the groove is too wide, the chips appear narrow, flow more freely, and do not deform sufficiently, making them difficult to break.
To achieve satisfactory chip breaking results, the appropriate width of the chip breaking groove should be selected according to specific processing conditions. For workpiece materials with lower hardness, the groove should be selected to be narrower; conversely, the groove should be selected to be wider.

TAG:


RELATED INFORMATION

ADD

Gengguantun Industrial Development Zone, Qingxian County, Hebei Province, China