【Summary】How to solve rust prevention and water seepage at weld seams of sheet metal products After acid washing and then phosphating and powder spraying at the weld seams of sheet metal processing, there will always be some rust water seeping out after a period of time. How should this problem be solved: 1. The acid at the seams during acid washing is not neutralized or is not completely neutralized, and the phosphating treatment does not form a complete film, which is prone to rust. After coating for a period of time, rust spreads and overflows from the seams. 2. Strong acid acid washing and strong alkaline degreasing treatment. The agents remaining at the seams neutralize each other and are not washed clean. After drying, there are white by-products at the seams. After a period of coating, these white by-products react chemically with corrosive media in the air and overflow from the seams. This problem often occurs between March and November. Manufacturers of sports equipment and office furniture should pay attention. This is a non-safe period. Careful pre-treatment is required. 2. Solutions to prevent rust in sheet metal processing: 1. Degreasing should use weak alkaline degreasing. It must not contain flake alkali components. TAL should be controlled at around 15 POINT. PH should not exceed 13. 2. Sulfuric acid can also be used for acid washing. The acid washing time should not be too long. Phosphoric acid is best used. 3. It is best to neutralize with 1-2 sodium carbonate after acid washing. 4. Surface adjustment is best done with oxalic acid, using a concentration of 1-2. 5. The acidity of zinc phosphating treatment should take the upper limit. Immersion treatment concentration: TA: above 35. FA: 1.2 AC: 8 (20CC fermentation tube) 6. All water washing processes must be cleaned thoroughly, and water washing should maintain overflow.
How to solve rust prevention and water seepage at weld seams of sheet metal products
After acid washing the weld seams of sheet metal processing and then phosphating and powder spraying, there will always be some rust water seeping out after a period of time. How should this problem be solved?
1. The acid in the crevice during acid washing is not neutralized or is not completely neutralized, and the phosphating treatment does not form a complete film, which is prone to rust. After coating for a period of time, rust spreads and overflows from the crevice.
2. Strong acid acid washing and strong alkaline degreasing treatment. The agents remaining in the crevice are not washed clean after mutual neutralization. After drying, there are white substances in the crevice. After a period of coating, these white substances react chemically with corrosive media in the air and overflow from the crevice.
This problem often occurs between March and November. Manufacturers of general sports equipment and office furniture should pay attention. This is a non-safe period. Careful pre-treatment is required.
Second, solutions to prevent rust in sheet metal processing:
1. Degreasing should use weak alkaline degreasing. It must not contain flake alkali components. TAL should be controlled around 15 POINT. PH should not exceed 13.
2. Sulfuric acid can also be used for acid washing. The acid washing time should not be too long. Phosphoric acid is best used.
3. It is best to neutralize with 1-2 sodium carbonate after acid washing.
4. Surface adjustment is best done with oxalic acid, using a concentration of 1-2.
5. The acidity of zinc phosphating treatment should take the upper limit. Immersion treatment concentration: TA: above 35. FA: 1.2 AC: 8 (20CC fermentation tube)
6. All washing processes must be cleaned thoroughly, and the washing should maintain overflow.