Issues to pay attention to in sheet metal design
Release time:
2021-12-11
【Summary】A. Bending interference issues; B. Minimum bend edge: not less than 4 times the plate thickness; going below this limit may greatly increase processing difficulty, or even make processing impossible. C. Deformation of holes caused by bending: holes too close to the bending line may be deformed by the mold. Since bending often needs to be determined based on actual conditions, maintaining necessary communication with process engineers can greatly improve design efficiency. 3. General Punching Where possible, standardize and unify to reduce mold costs and shorten sampling cycles. 4. Fitting Counterbore: It should be noted that the plate thickness should not be less than the height of the countersunk screw head; otherwise, the screw head will protrude above the plate, leading to an insecure fixation. 5. Riveting 5.1 When the plate thickness is less than 1mm, it may lead to easy detachment of the riveted parts; at this time, expanding rivets or welding after riveting can be used to ensure fastening strength. 5.2 The relationship between rivet screws and plate thickness Image 5.3 If the riveted part is too close to the edge, it will produce two consequences: A. The edge of the plate will deform after riveting (the edge will bulge), and the hole position will shift 0.1-0.5mm towards the edge; B. If the riveting position is too close to the bend edge, the upper mold cannot be pressed down: the distance from the outer edge of the riveting head to the bend edge should be no less than 3mm. 5.4 For U-shaped bent parts, the inner side riveting should consider whether the lower riveting mold can fit the workpiece; for other workpieces with relatively narrow internal spaces that require inner side riveting, this issue should be taken into account. 5.5 The specifications of riveted parts should be as uniform as possible to facilitate supplier ordering, shorten sampling cycles, and reduce the probability of errors in riveted parts. 6. Welding 6.1 For workpieces with relatively narrow internal spaces that require inner side welding, consideration should be given to how the welding gun can be inserted. 6.2 When the plate thickness is ≤1mm, it is easy to produce shrink holes or burn-through after welding, and the deformation caused by welding is relatively large. 6.3 Welding of materials such as copper and aluminum is more difficult and requires a higher skill level from welders. 7. Spraying Spraying is mainly divided into the following three types (each includes indoor and outdoor): Flat: can be subdivided into matte, flat, and glossy; the spraying layer thickness is about 60-90μm, and after recoating, it is about 90-120μm. Sand texture: can be subdivided into fine sand texture and coarse sand texture; the spraying layer thickness is about 50-80μm, and after recoating, it is about 80-110μm. Orange peel: can be subdivided into small orange peel and large orange peel; the spraying layer thickness is about 90-120μm, and after recoating, it is about 120-150μm. The spraying layer thickness in areas prone to powder accumulation will exceed the above thickness. 7.1 Flat: Advantages: aesthetically pleasing appearance, good silk screen effect; Disadvantages: high spraying cost, high rework rate, easily scratched, and surface scratches cannot be repaired, with glossy spraying being the most difficult. Avoid using flat finishes where possible, especially for large enclosures, as they are prone to bumps during handling. 7.2 Sand texture: Advantages: not easily scratched, spraying cost is the lowest among the three; Disadvantages: surface oil stains are not easy to remove, and silk screen effect is not as good as flat or orange peel. 7.3 Orange peel: Advantages: not easily scratched, good silk screen effect, surface oil stains are easy to remove, spraying cost is slightly higher than sand texture but far lower than flat. Disadvantages: aesthetic level is slightly lower than flat. 7.4 Spraying colors should be as uniform as possible, using the colors of the company's mainstream products to facilitate supplier ordering of powders. 7.5 A product should ideally use only one spraying color to reduce spraying costs (using multiple colors greatly increases processing time) and also reduce the probability of supplier spraying errors. 7.6 Avoid using silver powder. Silver powder contains silver compounds, and the price of the powder is twice that of ordinary powder, with greater spraying difficulty, leading to a higher likelihood of defects.
Issues to pay attention to in sheet metal design
A. Interference issues in bending;
B,Minimum bend allowance: Not less than 4 times the thickness of the plate; falling below this limit may greatly increase processing difficulty, or even make processing impossible.
C. Deformation of holes caused by bending: If the hole is too close to the bend line, it may be deformed by the mold.
Since bending often needs to be determined based on actual conditions, maintaining necessary communication with process engineers can greatly improve design efficiency.
3. Standard Punching
Where possible, standardize and unify to reduce mold costs and shorten sampling cycles.
4. Machining
Counterbore: It should be noted that the plate thickness is not less than the height of the countersunk screw head; otherwise, the screw head will protrude above the plate, leading to an insecure fixation.
5. Riveting
5.1 When the plate thickness is less than 1mm, it may lead to easy detachment of the riveted parts; at this time, bulging rivets can be used, or after rivetingWelding, to ensure fastening strength.
5.2 The relationship between rivet screws and plate thickness
5.3 If the riveted part is too close to the edge, it will produce two consequences:
A. The edge of the plate will deform after riveting (the edge will bulge), and the hole position will shift 0.1-0.5mm towards the edge; B. If the riveting position is too close to the bend edge, the upper mold of the riveting cannot be pressed down: the distance from the outer edge of the riveting head to the bend edge: not less than 3mm.
5.4 For U-shaped bent parts, the inner side riveting should consider whether the riveting lower mold can fit the workpiece; for other workpieces with relatively narrow internal spaces that require inner side riveting, this issue should be considered.
5.5 The specifications of riveted parts should be as uniform as possible to facilitate supplier ordering, shorten sampling cycles, and reduce the probability of errors in riveted parts.
6. Welding
6.1 For workpieces with relatively narrow internal spaces that require inner welding, consideration should be given to how the welding gun can be inserted. 6.2 When the plate thickness is ≤1mm, it is easy to produce shrink holes or burn-through after welding, and the deformation caused by welding is relatively large. 6.3 Welding of materials such as copper and aluminum is more difficult and requires a higher skill level from welders. 7,Spraying
Spraying is mainly divided into the following three types (each of which includes indoor and outdoor):
Flat finishIt can be categorized into matte, satin, and glossy finishes; the thickness of the spray coating is approximately 60-90μm, and after recoating, it is about 90-120μm.
Sand texture: It can be categorized into fine sand texture and coarse sand texture; the thickness of the spray coating is approximately 50-80μm, and after recoating, it is about 80-110μm.
Orange peel: It can be categorized into small orange peel and large orange peel; the thickness of the spray coating is approximately 90-120μm, and after recoating, it is about 120-150μm.
The spraying layer thickness in areas prone to powder accumulation will exceed the above thickness.
7.1 Flat finish: Advantages: Aesthetically pleasing, good silk screen effect; Disadvantages: High spraying cost, high rework rate, easily scratched, and surface scratches cannot be repaired, with high gloss being the most difficult to spray. Avoid using flat finishes where possible, especially for large enclosures, as they are prone to bumps during handling.
7.2 Sand texture: Advantages: Not easily scratched, spraying cost is the lowest among the three; Disadvantages: Surface oil stains are not easy to remove, and silk screen effect is not as good as flat or orange peel.
7.3 Orange peel: Advantages: Not easily scratched, good silk screen effect, surface oil stains are easy to remove, spraying cost is slightly higher than sand texture but far lower than flat finish. Disadvantages: Aesthetic degree is slightly lower than flat finish.
7.4 Spraying colors should be as uniform as possible, using the colors of the company's mainstream products to facilitate supplier ordering.
7.5 A product should ideally use only one spraying color to reduce spraying costs (using multiple colors greatly increases processing time) and also reduce the probability of spraying errors by suppliers.
7.6 Avoid using silver powder. Silver powder contains silvercompounds, and the powder price is twice that of ordinary powder, with greater spraying difficulty, easily leading to defects.
TAG:
RELATED INFORMATION
FAX
ADD
Gengguantun Industrial Development Zone, Qingxian County, Hebei Province, China
WeChat applet